Filter
By popularity (ascending)
By popularity (ascending)
Fraction of aggregate (at the customer's choice)
up to 0.7 mm; up to 3.2 mm
Temperature of working surface
from +5ºС to +30ºС
Compression resistance after 28 day storage
not less than 20 Mpa
Dry reinforced mixes for shotcreting and concrete spraying
By order
Fraction of aggregate (at the customer's choice)
up to 0.7 mm; up to 3.2 mm
Temperature of working surface
from +5ºС to +30ºС
Compression resistance after 28 day storage
not less than 30 Mpa
Dry reinforced mixes for shotcreting and concrete spraying
By order
Fraction of aggregate (at the customer's choice)
up to 0.7 mm; up to 3.2 mm
Temperature of working surface
from +5ºС to +30ºС
Compression resistance after 28 day storage
not less than 40 Mpa
Dry reinforced mixes for shotcreting and concrete spraying
By order
Fraction of aggregate (at the customer's choice)
up to 3.2 mm
Temperature of working surface
from +5ºС to +30ºС
Compression resistance after 28 day storage
not less than 50 Mpa
Dry reinforced mixes for shotcreting and concrete spraying
By order